600 MW机组凝汽器不锈钢管腐蚀原因分析
常亮,王锋涛,张小霓,王卫军,薛昌刚,王超煜
Analysis on the corrosion causes of stainless steel tubes in condensers of 600 MW unit
Liang Chang,Fengtao Wang,Xiaoni Zhang,Weijun Wang,Changgang Xue,Chaoyu Wang
表4
循环水运行监测数据
取样时间
pH
碱度/(mmol·L
-1
)
总硬度/(mmol·L
-1
)
Cl
-
/(mg·L
-1
)
2017-03-27
8.25
4.5
13.0
260
2017-03-07
8.56
5.6
14.8
346
2017-03-01
8.89
4.6
14.1
308
2017-02-24
8.42
4.5
13.2
258
2017-02-13
8.56
7.7
11.3
222
2017-02-07
8.42
7.8
11.3
232
2017-01-24
8.50
7.1
9.2
282
2017-01-17
8.58
7.3
9.2
256
2017-01-03
8.48
7.1
14.7
282
2016-12-27
9.42
8.5
14.3
253