不同热解温度生物炭对溶液中镉的吸附性能研究
|
王道涵,李景阳,汤家喜
|
Adsorption of cadmium in solution by biochar at different pyrolysis temperatures
|
Daohan Wang,Jingyang Li,Jiaxi Tang
|
|
表2 不同热解温度下3种生物炭等温吸附拟合结果
|
|
|
热解温度 | 生物炭型号 | Langmuir | | Freundlich | KL | Qm/(mg·g-1) | R2 | KF | n | R2 | 450 ℃ | Y1 | 0.026 36 | 10.074 43 | 0.984 43 | | 0.771 17 | 2.028 19 | 0.961 38 | S1 | 0.029 69 | 12.851 70 | 0.997 22 | 0.996 68 | 1.986 37 | 0.977 24 | H1 | 0.182 58 | 17.995 77 | 0.989 10 | 4.606 63 | 3.047 67 | 0.925 27 | 550 ℃ | Y2 | 0.108 84 | 14.530 67 | 0.987 21 | 2.831 92 | 2.608 72 | 0.977 84 | S2 | 0.299 11 | 15.231 95 | 0.946 87 | 5.111 92 | 3.712 09 | 0.952 59 | H2 | 1.840 50 | 19.611 63 | 0.968 14 | 9.842 58 | 4.459 11 | 0.943 69 | 650 ℃ | Y3 | 0.248 81 | 12.140 73 | 0.987 17 | 3.716 85 | 3.592 73 | 0.965 36 | S3 | 0.273 67 | 17.009 57 | 0.981 18 | 5.118 70 | 3.335 56 | 0.937 22 | H3 | 6.628 90 | 19.449 53 | 0.943 50 | 10.559 64 | 4.264 76 | 0.922 65 |
|
|
|