| IA-MA-AMPS共聚物的微波合成及其阻垢缓蚀研究
 | 
		
		| 杨武魁,袁小静,张黎黎,董社英 | 
			
			| Microwave synthesis IA-MA-AMPS copolymer and its scale and corrosion inhibition
 | 
		
		| Wukui Yang,Xiaojing Yuan,Lili Zhang,Sheying Dong | 
	
		|  | 
	
		| 表1 正交实验 
 | 
	
		|  | 
	
		|  | 
	
		| | 序号 | n(IA):n(MA):n(AMPS) | 阻垢率/% | 缓蚀率/% |  | IA | MA | AMPS |  | 1 | 1 | 1 | 1 | 92.45 | 91.23 |  | 2 | 1 | 2 | 2 | 75.63 | 73.09 |  | 3 | 1 | 3 | 3 | 89.19 | 87.61 |  | 4 | 2 | 1 | 2 | 78.63 | 76.75 |  | 5 | 2 | 2 | 3 | 72.05 | 73.72 |  | 6 | 2 | 3 | 1 | 82.35 | 81.36 |  | 7 | 3 | 1 | 3 | 78.93 | 78.23 |  | 8 | 3 | 2 | 1 | 87.36 | 83.16 |  | 9 | 3 | 3 | 2 | 79.08 | 80.17 |  | K1 | 85.76 | 83.34 | 87.39 | 阻垢率作为指标 |  | K2 | 77.68 | 78.35 | 77.78 |  | K3 | 81.79 | 83.24 | 80.06 |  | R | 8.08 | 5.19 | 9.61 |  | K1 | 83.98 | 82.07 | 85.25 | 缓蚀率作为指标 |  | K2 | 77.28 | 76.66 | 76.67 |  | K3 | 80.52 | 82.05 | 79.85 |  | r | 6.7 | 6.39 | 8.58 | 
 | 
	
		|  | 
	
		|  |