以聚苯胺制备富含氮多孔碳催化氧化降解酸性红73
宋翔,邢波,杨郭,袁基刚,刘兴勇

Degradation of acid red 73 by catalytic oxidation using nitrogen-rich porous carbon based on polyaniline preparation
Xiang Song,Bo Xing,Guo Yang,Jigang Yuan,Xingyong Liu
表1 不同造孔剂制得的富含氮多孔碳的比表面积及结构性质
催化剂 SBET/(m2·g-1 Vt/(cm3·g-1 Vmeso/(cm3·g-1 Vmeso/Vt/% D/nm
PANI-Na 48.5 0.281 0.278 98.9 22.91
PANI-K 46.5 0.328 0.323 98.4 27.68
PANI-Mg 51.5 0.470 0.460 97.9 35.69
PANI-Ca 124.9 0.492 0.487 98.9 18.84