泡沫镍阴极的循环冷却水电化学软化性能研究 |
陈东,曹顺安,蒋星明,董毕承 |
Electrochemical softening performance of nickel foam cathode in circulating cooling water |
Dong CHEN,Shun'an CAO,Xingming JIANG,Bicheng DONG |
图7 工作24 h后(a)和再生20 min后(b)泡沫镍表面的SEM图片 |
Fig.7 SEM images of the nickel foam surface after 24 h operation(a) and 20 min regeneration(b) |
![]() |