Catalytic degradation of tetracycline hydrochloride with persulfate catalyzed by composite of carbon and steel slag
|
Yan HUANG,Bo XING,Guo YANG,Qiang ZHOU,Zhongcai PAN
|
|
表2 不同GZ/AC复合材料的主要成分及其含量
|
Table 2 Composition of GZ/AC catalysts
|
|
样品 | 主要成分/% |
---|
Fe2O3 | SiO2 | CaO | ZnO | CuO | Al2O3 | MnO | MgO | P2O5 | TiO2 |
---|
GZ | 56.66 | 13.80 | 11.04 | 4.40 | 3.59 | 2.71 | 0.63 | 0.63 | 0.57 | 0.50 | 80%GZ/AC | 55.40 | 13.70 | 11.75 | 4.16 | 3.40 | 2.46 | 0.59 | 0.61 | 1.13 | 0.68 | 60%GZ/AC | 54.92 | 14.60 | 11.69 | 3.97 | 3.12 | 2.56 | 0.57 | 0.47 | 1.25 | 0.73 | 40%GZ/AC | 52.66 | 15.30 | 12.00 | 3.86 | 3.19 | 3.04 | 0.50 | 0.69 | 1.56 | 0.83 | 20%GZ/AC | 51.15 | 16.10 | 12.60 | 3.25 | 2.43 | 3.00 | 0.46 | 0.34 | 2.21 | 1.02 | AC | 2.96 | 1.48 | 0.97 | — | — | 0.22 | — | — | 0.26 | 0.21 |
|
|
|