不锈钢水冷器应力腐蚀开裂原因探讨

齐冬子   

  1. 原化学工业部化肥司, 北京 100031
  • 收稿日期:2008-04-16 修回日期:2008-04-16 出版日期:2008-09-20 发布日期:2010-10-01
  • 作者简介:齐冬子(1929- ),1935年毕业于大连工学院化工系,原化工部化肥司教授级高级工程师。联系电话:010-66014605。

Discussion on reasons of stress corrosion cracks in stainless steel water cooler

Qi Dongzi   

  1. Department of Chemical Fertilizer, Former Ministry of Chemical Industry, Beijing 100031, China
  • Received:2008-04-16 Revised:2008-04-16 Online:2008-09-20 Published:2010-10-01

摘要:

根据化肥厂中不锈钢水冷器损坏情况,分析了导致不锈钢水冷器应力腐蚀开裂的诸因素,指出循环冷却水中氯离子的含量并不是应力腐蚀开裂的决定性因素,水冷器的出水温度是重要因素。

关键词: 不锈钢, 循环冷却水, 腐蚀开裂

Abstract:

Based on the damages of stainless water coolers in chemical fertilizer plants, the influential factors of the stress corrosion cracks are analyzed. The effluent water temperature of the water cooler is an important factor.

Key words: stainless steel, circulating cooling water, corrosion cracks