Characteristics of oxidation and decomposition of strong acidic cation exchange resin in hydrogen peroxide

Zhu Zhiping, Zhou Yu, Zhao Yongfu, Guo Xiaocui   

  1. Changsha University of Science & Technology, Changsha 410004, China
  • Received:2012-07-09 Online:2012-09-20 Published:2012-09-20

强酸阳树脂在过氧化氢中的氧化分解特性研究

朱志平, 周瑜, 赵永福, 郭小翠   

  1. 长沙理工大学, 湖南长沙 410004
  • 作者简介:朱志平(1963-),教授,博士。E-mail:zzp8389@163.com
  • 基金资助:

    大型先进压水堆核电站重大专项支持(2011ZX06004-017)

Abstract:

SO42- may cause intergranular stress corrosion cracking of nickel-based metal in nuclear power stations, resulting in serious hazards to the economically running of the nuclear power stations. To explore the source of SO42- of nuclear power stations,dynamic dissolving characteristics of several kinds of imported cation exchange resins in hydrogen peroxide solution have been researched. The dissolved liquid of SO42-,TOC are determined by ion chromatography and TOC meter. The results show that the effects of hydrogen peroxide on macro-porous resin and geltype resin are different. The higher the oxidant concentration is,the higher the influence on resin is,and the more SO42- is dissolved. And it is very likely that the desulfonation rate decreases with time,and the change of dissolving rate of organisms is relatively small.

Key words: strong acidic cation exchange resin, hydrogen peroxide, dynamic dissolution, nuclear power station

摘要:

在核电站,SO42-会引起镍基金属的晶间应力腐蚀破裂,对核电站的安全经济运行造成严重危害.为探索核电站SO42-的来源,研究了几种进口阳树脂在H2O2溶液中的动态溶出特性,采用离子色谱仪和TOC仪对溶出液的SO42-、TOC进行测定.研究结果表明,过氧化氢对大孔型和凝胶型树脂的影响不同,且氧化剂浓度越高,对树脂的影响越大,溶出的SO42-也越多;脱磺化速率随着时间推移而降低,而有机物溶出速率变化相对较小.

关键词: 强酸型阳离子交换树脂, 过氧化氢, 动态溶出, 核电站