INDUSTRIAL WATER TREATMENT ›› 2011, Vol. 31 ›› Issue (8): 38-41. doi: 10.11894/1005-829x.2011.(31).8.38

Previous Articles     Next Articles

Preparation of coal gauge based PSFA and its application to the treatment of drilling wastewater

Wang Huiyun1, Quan Xiangao1, Shi Maojian1, Wang Jun2   

  1. 1. Pharmaceutical College, Jining Medical University, Rizhao 276826, China;
    2. Enhanced Oil Recovery Research Center, China University of Petroleum, Beijing 102249, China
  • Received:2011-05-02 Revised:2011-05-02 Online:2011-08-20 Published:2011-08-29

矸石基PSFA的制备及其对钻井废水的处理

王慧云1, 全先高1, 石茂建1, 王军2   

  1. 1. 济宁医学院药学院, 山东日照 276826;
    2. 中国石油大学(北京)提高采收率中心, 北京102249
  • 作者简介:王慧云(1968- ),2005 年毕业于中国石油大学(北京),博士,教授,从事胶体界面化学研究。电话:0633-8108287,E-mail:wang_huiyun@126.com。
  • 基金资助:

    国家十一五科技支撑项目(2008BAC43B02)

Abstract:

Polyaluminum ferric silicate(PSFA) flocculant has been prepared by using coal gauge as raw material. The effects of pH,n (Si)∶n (Al+Fe) on the flocculating capacity of the coal gauge based flocculant polyaluminum ferric silicate are investigated. The result indicates that in the process of ignition under high temperature,the transformation of crystalline structure takes place. The flocculant prepared by adding acid extracting solution into base extracting solution and pressurizing has optimum flocculating capacity. The infra-red spectrum shows that the atoms Si,Al,Fe in the PSAF prepared are polymerized,and the optimization conditions for the flocculant are as follows: n(Si)∶n(Al+Fe)=1∶1,and pH is 3-4. Thus,the COD removal rate is more than 95% when it is applied to the treatment of drilling wastewater from Shengli Oilfield.

Key words: coal gauge, polyaluminum ferric silicate, flocculant

摘要:

以煤矸石为原料制备了聚硅铝铁(PSFA)絮凝剂。考察了pH、n(Si):n(Al+Fe)对矸石基聚硅铝铁絮凝剂絮凝能力的影响。结果表明:在高温灼烧过程中煤矸石的晶型结构发生了变化,采用向碱提取液中加入酸提取液并加压的方式制得的絮凝剂具有最佳絮凝效果。红外光谱表明所制得的聚硅铝铁絮凝剂中硅、铝、铁均以聚合态存在。当n(Si):n(Al+Fe)=1:1,pH在3~4时为其最佳絮凝条件,用于胜利油田钻井废水处理时,COD去除率>95%。

关键词: 煤矸石, 聚硅铝铁, 絮凝剂

CLC Number: