工业水处理 ›› 2020, Vol. 40 ›› Issue (9): 49-53. doi: 10.11894/iwt.2019-0941

• 试验研究 • 上一篇    下一篇

离子液体辅助燃烧法制备多孔La2O3及其吸附性能研究

赵金花1(),王宇松2,傅韬1,黄忠亮1,陈武华1,欧阳清海1,吕芬芬1,罗江水3,*()   

  1. 1. 龙岩学院化学与材料学院, 福建龙岩 364000
    2. 龙岩学院物理与机电工程学院, 福建龙岩 364000
    3. 四川大学材料科学与工程学院, 四川成都 610065
  • 收稿日期:2020-07-12 出版日期:2020-05-20 发布日期:2020-10-21
  • 通讯作者: 罗江水 E-mail:zjh1979good@163.com;jiangshui.luo@gmail.com
  • 作者简介:赵金花(1979-),高级实验师。E-mail:zjh1979good@163.com
  • 基金资助:
    国家自然科学基金委面上项目(21776120);福建省自然科学基金项目(2018J01433);龙岩学院校产学研项目(LC20160002);龙岩市科技计划项目(2017LY89)

Preparation of porous cerium oxide synthesized by low temperature combustion method assisted by ionic liquid and its adsorption properties analysis

Jinhua Zhao1(),Yusong Wang2,Tao Fu1,Zhongliang Huang1,Wuhua Chen1,Qinghai Ouyang1,Fenfen Lü1,Jiangshui Luo3,*()   

  1. 1. College of Chemistry and Materials, Longyan University, Longyan 364000, China
    2. College of Physics and Mechanical&Electrical Engineering, Longyan University, Longyan 364000, China
    3. College of Materials Science and Engineering, Sichuan University, Chengdu 610065, China
  • Received:2020-07-12 Online:2020-05-20 Published:2020-10-21
  • Contact: Jiangshui Luo E-mail:zjh1979good@163.com;jiangshui.luo@gmail.com

摘要:

以六水硝酸镧和甘油为原料,聚乙二醇为分散剂,N-甲基-N-苄基吗啉离子液体作为辅助试剂,采用低温燃烧合成法制备La2O3粉体。利用XRD、STA、BET、SEM对La2O3进行表征。结果表明,所制备的La2O3为多孔结构、热稳定性良好、结晶度和纯度均较好,同时测试了多孔La2O3的吸附性能,考察了PO43-初始浓度、溶液pH、吸附温度、吸附时间对吸附量的影响,在PO43-初始质量浓度为0.2 g/L,溶液pH为6,吸附温度为55℃,吸附时间为90 min的最优条件下,吸附量可达550.62 mg/g,PO43-在多孔La2O3表面的吸附符合准一级动力学模型,等温吸附过程符合Langmuir等温吸附模型。

关键词: 离子液体, 氧化镧, 低温燃烧法, N-甲基吗啉, 多孔结构

Abstract:

The lanthanum oxide powder was synthesized by low temperature combustion method using lanthanum nitrate hexahydrate and glycerin as raw materials, polyethylene glycol(CP) as dispersant and N-methyl-N-benzylmorpholine ionic liquid as auxiliary reagent. The La2O3 was characterized by XRD, STA, BET and SEM. The results showed that the prepared lanthanum oxide had a porous structure, good thermal stability, good crystallinity and purity. The adsorption of La2O3 was investigated. The effects of initial concentration of phosphate, pH of solution, adsorption temperature, and adsorption time on adsorption capacity were observed. The adsorption capacity could reach 550.62 mg/g under the optimum condition of the initial concentration of phosphate 0.2 g/L, pH 6, adsorption temperature 55℃, adsorption time 90 min. The adsorption of phosphate on the La2O3 meet to pseudo-first order kinetic model and the isothermal adsorption process conforms to Langmuir isothermal adsorption model.

Key words: ionic liquid, lanthanum oxide, low temperature combustion method, N-methyl morpholine, porous structure