INDUSTRIAL WATER TREATMENT ›› 2014, Vol. 34 ›› Issue (8): 29-31. doi: 10.11894/1005-829x.2014.34(8).029

Previous Articles     Next Articles

Treatment of effluent from micro-aerobic reactor by biological contact oxidation with steel-slag ceramisites

Liu Xiao, Yang Yong, Zhai Mei   

  1. Earthquake Engineering Research Center of Hebei Province, College of Civil and Architectural Engineering, Hebei United University, Tangshan 063009, China
  • Received:2014-07-10 Online:2014-08-20 Published:2014-08-25

钢渣陶粒生物接触氧化处理微氧出水的研究

刘晓, 杨永, 翟梅   

  1. 河北联合大学建筑工程学院, 河北省地震工程研究中心, 河北唐山 063009
  • 作者简介:刘晓(1976-),博士,讲师。电话:15027607001,E-mail:xiaoliu200401@163.com。
  • 基金资助:

    河北省科技计划项目(12273607);唐山市科学技术研究与发展计划(13130241z)

Abstract:

Steel-slag ceramisites have been made by using steel slag as their main raw material and adding a small amount of clay and pore-forming agent,and have been applied to biological contact oxidation process for treating micro-aerobic effluent. The results show that COD,nitrogen and phosphorus can be simultaneously removed by steel-slag ceramisites-biological contact oxidation process. When it runs steadily under the following conditions:contact oxidation time is 2.5 h,mass concentrations of influent COD,TP,NH4+-N and TN are 20-86,0.8-6.0,8.2-31.4,and 9.9-33.2 mg/L,respectively,the average mass concentrations of effluent COD,TP,NH4+-N and TN are 18,0.6,0.2 and 3.5 mg/L,respectively,meeting the requirements of the first class of Discharge Standard of Pollutants for Municipal Wastewater Treatment Plant(GB 18918-2002).

Key words: steel-slag ceramisite, biological contact oxidation, nitrogen removal, phosphorus removal

摘要:

以钢渣为主要原料,添加少量黏土和造孔剂制备钢渣陶粒,用于生物接触氧化处理微氧反应器出水。结果表明,钢渣陶粒生物接触氧化工艺能同时去除COD和脱氮除磷。在接触氧化时间为2.5 h,进水COD、TP、NH4+-N、TN的质量浓度分别为20~86、0.8~6.0、8.2~31.4、9.9~33.2 mg/L的条件下稳定运行,出水COD、TP、NH4+-N、TN的平均质量浓度分别为18、0.6、0.2、3.5 mg/L,满足GB 18918-2002的一级标准要求。

关键词: 钢渣陶粒, 生物接触氧化, 脱氮, 除磷