Industrial Water Treatment ›› 2019, Vol. 39 ›› Issue (10): 82-84. doi: 10.11894/iwt.2018-0799

• Research and Experiment • Previous Articles     Next Articles

Study on disposal and recovery process of a strong acidic waste liquid with high concentrations of arsenic and copper

Ying Wu(),Yanjie Yu,Dengzhi Fang,Shujun Xiao,Xiao Yan   

  1. Chinese People's Liberation Army 61699 Troops, Yichang 443000, China
  • Received:2019-07-18 Online:2019-10-20 Published:2019-10-29

某强酸性高浓度砷铜废液的处置及回收工艺研究

吴莹(),于艳杰,方登志,肖淑君,严霄   

  1. 中国人民解放军61699部队, 湖北宜昌 443000
  • 作者简介:吴莹(1989-),硕士,工程师。电话:18674209720, E-mail:415613010@qq.com

Abstract:

The arsenic content of the waste liquid in a resource recycling center is 142 000 mg/L, copper content is 15 800 mg/L, and pH < 0. The waste liquid was first reduced by NaHSO3 and then filtered. The filter residue was dried to obtain As2O3, while the filtrate was replaced by iron to obtain sponge copper. The process conditions for recycling As2O3 and copper were optimized by orthogonal test. The test results showed that under the best process conditions, the recovery rate of arsenic reached 95.0%, and the mass fraction of As2O3 reached 94.0%, the copper recovery rate reached 98.0%, and the mass fraction of copper in copper slag reached 90.5%. Both recycled As2O3 and copper slag met the industrial raw material standards. The waste liquid of recovered arsenic and copper met'Integrated Wastewater Discharge Standard'(GB 8978-1996) by subsequent processing.

Key words: waste liquid containing arsenic and copper, arsenic trioxide, copper, recovery

摘要:

某资源回收中心的废液中砷高达142 000 mg/L,铜为15 800 mg/L,废液pH < 0。该废液经NaHSO3还原、过滤、烘干可回收As2O3;所得滤液经铁置换可回收海绵铜。采用正交试验对As2O3、铜回收的工艺条件进行了优化。结果表明:在最佳工艺条件下,砷回收率达95.0%,所得As2O3质量分数达94.0%;铜回收率为98.0%,所得铜渣中铜质量分数达90.5%。回收所得As2O3、铜渣均达到工业原料标准。回收砷和铜的废液经后续处理后达到《污水综合排放标准》(GB 8978-1996)要求。

关键词: 含砷铜废液, 三氧化二砷, 铜, 回收